产品介绍 > 功率铁氧体颗粒料 |
|
| 材
料 系 列 名 称 |
RP2K5 |
RP2K3 |
RP2K4 |
RP1K4 |
RP1K8 |
| 初始磁导率
μi |
2500±25% |
2300±25% |
2400±25% |
1400±25% |
1400±25% |
磁芯损耗 Pc
mW/cm3 |
| (25kHz,200mT) |
25℃ |
| 60℃ |
| 80℃ |
|
130 |
120 |
|
|
|
| 90 |
80 |
|
|
|
| 100 |
70 |
|
|
|
| (100kHz,200mT) |
25℃ |
| 60℃ |
| 100℃ |
| 120℃ |
|
700 |
600 |
600 |
|
|
| 500 |
450 |
400 |
|
|
| 600 |
410 |
300 |
|
110 |
| |
500 |
380 |
|
|
| (500kHz,50mT) |
25℃ |
| 60℃ |
| 100℃ |
|
|
|
|
130 |
|
| |
|
|
80 |
|
| |
|
|
80 |
4.2(16kHz,150mT) |
饱和磁通密度(H=1194A/m)
Bs mT |
25℃ |
| 100℃ |
|
510 |
510 |
500 |
470(H=1600A/m) |
510 |
| 390 |
390 |
390 |
380 |
390 |
| 剩磁
Br mT 25℃ |
117 |
95 |
110 |
140 |
170 |
| 矫顽力
Hc A/m 25℃ |
14 |
14.3 |
13 |
36.5 |
16 |
| 居里温度
Tc/℃ |
230 |
215 |
215 |
240 |
240 |
| 表观密度
d g/cm3 |
4.8 |
4.8 |
4.8 |
4.8 |
4.8 |
| 电阻率
ρ Ω-m |
10 |
6.5 |
6.5 |
|
|
| 颗粒分布(40-180目) |
≥70% |
≥70% |
≥70% |
≥70% |
>70% |
| 松装比重
dB g/cm3 |
1.22-1.42 |
1.22-1.42 |
1.22-1.42 |
1.22-1.42 |
1.22-1.42 |
| 堆积角落
θ/。 |
≤30。 |
≤30。 |
≤30。 |
≤30。 |
≤30。 |
| 含水量
η/% |
≤0.5% |
≤0.5% |
≤0.5% |
≤0.5% |
≤0.5% |
| 注:以上数据由环形磁芯在室温下测得,若有特殊要求可另订协议 |
|